Logo Repositorio Institucional

Por favor, use este identificador para citar o enlazar este ítem: https://dspace.ucuenca.edu.ec/handle/123456789/37299
Título : Resistance to fracture of lithium disilicate feldspathic restorations manufactured using a CAD/CAM system and crystallized with different thermal units and programs
Autor: Abad Coronel, Cristian Gustavo
Ordoñez Balladares, Andrea Dolores
Fajardo Seminario, Jorge Isaac
Martín Biedma, Benjamín José
Correspondencia: Abad Coronel, Cristian Gustavo, cristian.abad@ucuenca.edu.ec
Palabras clave : Lithium disilicate
Crystallization
Fracture
CAD CAM
Materials
Área de conocimiento FRASCATI amplio: 3. Ciencias Médicas y de la Salud
Área de conocimiento FRASCATI detallado: 3.2.15 Odontología
Área de conocimiento FRASCATI específico: 3.2 Medicina Clínica
Área de conocimiento UNESCO amplio: 09 - Salud y Bienestar
ÁArea de conocimiento UNESCO detallado: 0911 - Estudios Dentales
Área de conocimiento UNESCO específico: 091 - Salud
Fecha de publicación : 2021
Volumen: Volumen 14, número 12
Fuente: Materials
metadata.dc.identifier.doi: 10.3390/ma14123215
Tipo: ARTÍCULO
Abstract: 
The aim of this study was to determine the resistance to fracture of feldspathic restorations with lithium disilicate and crystallized with different ovens and programs. Methods: Sixty monolithic restorations (LD) (EMAX CAD™ LT, Ivoclar-Vivadent™) were designed with the same parameters and milled with a CAD/CAM system (CEREC SW 5.1, CEREC MCXL, Dentsply-Sirona™, Bensheim). Each restoration was randomly assigned by randomization software (RANDNUM) to one of the three groups: (a) (NF) Oven P310 (Ivoclar, Vivadent) normal crystallization program, (b) (FF) Ivoclar P310 oven (Ivoclar-Vivadent™) rapid crystallization program, or (c) (SF) SpeedFire oven (DentsplySirona™). Results: There were statistically significant differences between the groups (ANOVA, p < 0.05). The NF and FF groups showed the highest values of resistance to fracture, with statistically significant differences with the SF group. Conclusions: Using a furnace from the same dental company with predetermined programs from the material manufacturer, as well as using a predetermined program for rapid crystallization, has no effect on fracture resistance, and would save clinical time when performing ceramic restorations with lithium disilicate, while keeping their mechanical properties.
URI : https://www.scopus.com/inward/record.uri?eid=2-s2.0-85108459870&doi=10.3390%2fma14123215&partnerID=40&md5=ca15b657a0f8596de58cb5d63f86dfb1
URI Fuente: https://www.mdpi.com/1996-1944/14/12
ISSN : 1996-1944
Aparece en las colecciones: Artículos

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
documento.pdfdocument1.6 MBAdobe PDFVista previa
Visualizar/Abrir


Este ítem está protegido por copyright original



Los ítems de DSpace están protegidos por copyright, con todos los derechos reservados, a menos que se indique lo contrario.

 

Centro de Documentacion Regional "Juan Bautista Vázquez"

Biblioteca Campus Central Biblioteca Campus Salud Biblioteca Campus Yanuncay
Av. 12 de Abril y Calle Agustín Cueva, Telf: 4051000 Ext. 1311, 1312, 1313, 1314. Horario de atención: Lunes-Viernes: 07H00-21H00. Sábados: 08H00-12H00 Av. El Paraíso 3-52, detrás del Hospital Regional "Vicente Corral Moscoso", Telf: 4051000 Ext. 3144. Horario de atención: Lunes-Viernes: 07H00-19H00 Av. 12 de Octubre y Diego de Tapia, antiguo Colegio Orientalista, Telf: 4051000 Ext. 3535 2810706 Ext. 116. Horario de atención: Lunes-Viernes: 07H30-19H00